Mar 01, 2020· The reducibility of titano magnetite iron ore materials (agglomerate, pellets) with vario us TiO 2 contents are studied TheThrough magnetite concentration deteriorates reducibility because of high FeO content in sinter product Such situation makes it to promote oxidation of magnetite iron ore during sintering process for improving sinter reducibility In addition, promoting oxidation of magnetite possibly increases sinter strength with using oxidation heatImprovement of Sinter Strength and Reducibility throughimproving reducibility of iron ore by adding metallic Ni containing materials wherein, the catalytic effect for the reduction was generated by the addition of metallic Ni Presence of Cr 3+ also increases the reducibility of iron oxide by CO due to catalytic effect of partially filled dband and unpaired electron [14 ]Improving reducibility of iron ore pellets by optimization
About 1kg of each ore, which was crushed to various size (maximum of 3 in), was treated at 900°C using 20l/min/kg of H 2 gas as a reducing medium The reduction degree was based on the total weight of oxygen which combined with the iron in ore, and measured by means of the lossinweight methodDec 01, 1973· Lime additions (with or without silica) lower the reducibility of sintered hematite and magnetite ore pellets When silica alone is added, the reducibility of the pellet is not much affected In the reduction of pellets made from a highgrade iron ore with no lime addition, there is initially rapid internal reduction of hematite to wustiteReducibility of iron ore pellets and effect of additionsPrior oxidation of magnetite ore to Fe 2 O 3 leads to similar reduction behavior when compared with natural hematite; however, natural magnetite is hardly reducible due to low porosity and the formation of dense intermediate products during the reduction 8) Accompanying oxides in the iron ore, such as alumina, influence the reduction rateReduction of Iron Oxides with Hydrogen—A Review
The reducibility of iron ore pellets of a specific chemistry can be improved by the optimization of physical parameters such as induration temperature, improving size distribution of fines高达10%返现· Apr 25, 2019· To improve the reducibility of titaniferous magnetite ore (TMO), a technique of hightemperature heating followed by water quenching has been adapted This quenching technique imparts cracks into the dense TMO which in turn leads to the enhancement of reducibility during carbothermal reduction using boiler grade coal A majorOptimization of Reduction Parameters of Quenched